MILL-MAX MFG CORP
|
| Part No. |
0908-5-15-20-75-14-11-0
|
| OCR Text |
...s as machined: 80-90 rockwell b density: .307 lbs/in3 electrical conductivity: 26% iacs* melting point: 900c/885c (liquidus/solidus) ?(3 to 4% lead is used to permit "free machining" and is permitted by ec directive 2002/95annex 6; so all p... |
| Description |
BERYLLIUM COPPER, GOLD (10) OVER NICKEL FINISH, PCB TERMINAL
|
| File Size |
100.58K /
2 Page |
View
it Online |
Download Datasheet
|
| |
|
 |
MILL-MAX MFG CORP
|
| Part No. |
0908-7-15-20-75-14-11-0
|
| OCR Text |
...s as machined: 80-90 rockwell b density: .307 lbs/in3 electrical conductivity: 26% iacs* melting point: 900c/885c (liquidus/solidus) ?(3 to 4% lead is used to permit "free machining" and is permitted by ec directive 2002/95annex 6; so all p... |
| Description |
BERYLLIUM COPPER, GOLD (10) OVER NICKEL FINISH, PCB TERMINAL
|
| File Size |
100.91K /
2 Page |
View
it Online |
Download Datasheet
|
| |
|
 |
MILL-MAX MFG CORP
|
| Part No. |
0950-0-15-20-71-14-11-0
|
| OCR Text |
...s as machined: 80-90 rockwell b density: .307 lbs/in3 electrical conductivity: 26% iacs* melting point: 900c/885c (liquidus/solidus) ?(3 to 4% lead is used to permit "free machining" and is permitted by ec directive 2002/95annex 6; so all p... |
| Description |
BRASS, GOLD (10) OVER NICKEL FINISH, PCB TERMINAL
|
| File Size |
93.98K /
2 Page |
View
it Online |
Download Datasheet
|
| |
|
 |
MILL-MAX MFG CORP
|
| Part No. |
2101-3-00-01-00-00-07-0
|
| OCR Text |
...s as machined: 80-90 rockwell b density: .307 lbs/in3 electrical conductivity: 26% iacs* melting point: 900c/885c (liquidus/solidus) ?(3 to 4% lead is used to permit "free machining" and is permitted by ec directive 2002/95annex 6; so all p... |
| Description |
BRASS, TIN LEAD (200) OVER NICKEL FINISH, PCB TERMINAL
|
| File Size |
88.56K /
2 Page |
View
it Online |
Download Datasheet
|
|

Price and Availability
|